Allgemein
Abmessung
Property | Value |
---|---|
Dicke | 6 - 575 mm Show Supplier Material materials with Dicke of 6 - 575 mm |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 20 % Show Supplier Material materials with Dehnung of 20 % |
Elastizitätsmodul | 23.0 °C | 69 GPa Show Supplier Material materials with Elastizitätsmodul of 69 GPa |
Härte, HBW | 23.0 °C | 20 [-] Show Supplier Material materials with Härte, HBW of 20 [-] |
Schubmodule | 23.0 °C | 25.9 GPa Show Supplier Material materials with Schubmodule of 25.9 GPa |
Streckgrenze | 23.0 °C | 28 MPa Show Supplier Material materials with Streckgrenze of 28 MPa |
Zugfestigkeit | 23.0 °C | 65 MPa Show Supplier Material materials with Zugfestigkeit of 65 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 2.35E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.35E-5 1/K | Mean values between 20°C and the mentioned temperature |
200.0 °C | 2.44E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.44E-5 1/K | Mean values between 20°C and the mentioned temperature | |
300.0 °C | 2.54E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.54E-5 1/K | Mean values between 20°C and the mentioned temperature | |
Spezifische Wärmekapazität | 23.0 °C | 900 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 900 J/(kg·K) | |
Wärmeleitfähigkeit | 23.0 °C | 210 - 220 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 210 - 220 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 3.40E+7 - 3.60E+7 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 3.40E+7 - 3.60E+7 S/m |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | Balance | ||
Andere | 0.03 % Show Supplier Material materials with Andere of 0.03 % | Single | |
Eisen | 0.4 % Show Supplier Material materials with Eisen of 0.4 % | ||
Kupfer | 0.05 % Show Supplier Material materials with Kupfer of 0.05 % | ||
Magnesium | 0.05 % Show Supplier Material materials with Magnesium of 0.05 % | ||
Mangan | 0.05 % Show Supplier Material materials with Mangan of 0.05 % | ||
Silizium | 0.25 % Show Supplier Material materials with Silizium of 0.25 % | ||
Titan | 0.05 % Show Supplier Material materials with Titan of 0.05 % | ||
Zink | 0.07 % Show Supplier Material materials with Zink of 0.07 % |
Technological properties
Property | ||
---|---|---|
Anodizing | very good | |
Application areas | Electronics industry; Semiconductor industry; Panelling in machine construction and plant construction; Parts with a decorative surface; Automotive parts; Food industry | |
Corrosion properties | good | |
Dimensional stability | very good | |
General machinability | very good | |
Soldering general | very good | |
Welding | Gas: good, WIG: good |