Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.66 g/cm³ Show Supplier Material materials with Dichte of 2.66 g/cm³ |
Oberflächenrauigkeit | 0.4 μm Show Supplier Material materials with Oberflächenrauigkeit of 0.4 μm |
Abmessung
Property | Value |
---|---|
Dicke | 6 - 1000 mm Show Supplier Material materials with Dicke of 6 - 1000 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 15 % Show Supplier Material materials with Dehnung of 15 % | A10 mm |
Elastizitätsmodul | 23.0 °C | 70 GPa Show Supplier Material materials with Elastizitätsmodul of 70 GPa | |
Härte, HBW | 23.0 °C | 70 - 80 [-] Show Supplier Material materials with Härte, HBW of 70 - 80 [-] | |
Streckgrenze | 23.0 °C | 110 - 130 MPa Show Supplier Material materials with Streckgrenze of 110 - 130 MPa | |
Zugfestigkeit | 23.0 °C | 230 - 290 MPa Show Supplier Material materials with Zugfestigkeit of 230 - 290 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 2.35E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.35E-5 1/K | Mean values between 20°C and the mentioned temperature |
Spezifische Wärmekapazität | 23.0 °C | 900 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 900 J/(kg·K) | |
Wärmeleitfähigkeit | 23.0 °C | 110 - 140 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 110 - 140 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 1.60E+7 - 1.80E+7 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 1.60E+7 - 1.80E+7 S/m |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | Balance | ||
Andere | 0.15 % Show Supplier Material materials with Andere of 0.15 % | Total | |
Chrom | 0.05 - 0.25 % Show Supplier Material materials with Chrom of 0.05 - 0.25 % | ||
Eisen | 0.4 % Show Supplier Material materials with Eisen of 0.4 % | ||
Kupfer | 0.1 % Show Supplier Material materials with Kupfer of 0.1 % | ||
Magnesium | 4 - 4.9 % Show Supplier Material materials with Magnesium of 4 - 4.9 % | ||
Mangan | 0.4 - 1 % Show Supplier Material materials with Mangan of 0.4 - 1 % | ||
Silizium | 0.4 % Show Supplier Material materials with Silizium of 0.4 % | ||
Titan | 0.15 % Show Supplier Material materials with Titan of 0.15 % | ||
Zink | 0.25 % Show Supplier Material materials with Zink of 0.25 % |
Technological properties
Property | ||
---|---|---|
Anodizing | good | |
Application areas | Tool making, mould making and model making; Blow moulds and injection moulds; Laminating tools; Moulds for elastomer materials; Moulds and heat-stressed parts; Moulds with welded construction; Refrigeration technology | |
Corrosion properties | very good | |
Dimensional stability | very good | |
General machinability | very good | |
Welding | WIG: good, MIG: good, Resistance welding: good |