Allgemein
Abmessung
Property | Value |
---|---|
Dicke | 8 - 100 mm Show Supplier Material materials with Dicke of 8 - 100 mm |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 5 - 6 % Show Supplier Material materials with Dehnung of 5 - 6 % |
Dehnung A50 | 23.0 °C | 7 % Show Supplier Material materials with Dehnung A50 of 7 % |
Elastizitätsmodul | 23.0 °C | 72 GPa Show Supplier Material materials with Elastizitätsmodul of 72 GPa |
Härte, HBW | 23.0 °C | 126 - 140 [-] Show Supplier Material materials with Härte, HBW of 126 - 140 [-] |
Streckgrenze | 23.0 °C | 340 - 390 MPa Show Supplier Material materials with Streckgrenze of 340 - 390 MPa |
Zugfestigkeit | 23.0 °C | 430 - 475 MPa Show Supplier Material materials with Zugfestigkeit of 430 - 475 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 2.34E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.34E-5 1/K | Mean values between 20°C and the mentioned temperature |
200.0 °C | 2.43E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.43E-5 1/K | Mean values between 20°C and the mentioned temperature | |
300.0 °C | 2.52E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.52E-5 1/K | Mean values between 20°C and the mentioned temperature | |
Spezifische Wärmekapazität | 23.0 °C | 862 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 862 J/(kg·K) | |
Wärmeleitfähigkeit | 23.0 °C | 130 - 160 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 130 - 160 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 1.90E+7 - 2.30E+7 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 1.90E+7 - 2.30E+7 S/m |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | Balance | ||
Andere | 0.15 % Show Supplier Material materials with Andere of 0.15 % | Total | |
Chrom | 0.18 - 0.28 % Show Supplier Material materials with Chrom of 0.18 - 0.28 % | ||
Eisen | 0.5 % Show Supplier Material materials with Eisen of 0.5 % | ||
Kupfer | 1.2 - 2 % Show Supplier Material materials with Kupfer of 1.2 - 2 % | ||
Magnesium | 2.1 - 2.9 % Show Supplier Material materials with Magnesium of 2.1 - 2.9 % | ||
Mangan | 0.3 % Show Supplier Material materials with Mangan of 0.3 % | ||
Silizium | 0.4 % Show Supplier Material materials with Silizium of 0.4 % | ||
Titan | 0.2 % Show Supplier Material materials with Titan of 0.2 % | ||
Zink | 5.1 - 6.1 % Show Supplier Material materials with Zink of 5.1 - 6.1 % |
Technological properties
Property | ||
---|---|---|
Anodizing | moderate | |
Application areas | Tool making, mould making and model making; Aerospace; Military technology | |
Corrosion properties | moderate | |
General machinability | good | |
Soldering general | not recommended | |
Welding | Resistance welding: good |