Abmessung
Property | Value |
---|---|
Dicke | 10 mm Show Supplier Material materials with Dicke of 10 mm |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 8 % Show Supplier Material materials with Dehnung of 8 % |
Dehnung A50 | 23.0 °C | 6 % Show Supplier Material materials with Dehnung A50 of 6 % |
Härte, Brinell | 23.0 °C | 75 [-] Show Supplier Material materials with Härte, Brinell of 75 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 170 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 170 MPa |
Zugfestigkeit | 23.0 °C | 215 MPa Show Supplier Material materials with Zugfestigkeit of 215 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | balance |
Andere | 0.05 - 0.15 % Show Supplier Material materials with Andere of 0.05 - 0.15 % |
Chrom | 0.1 % Show Supplier Material materials with Chrom of 0.1 % |
Eisen | 0.35 % Show Supplier Material materials with Eisen of 0.35 % |
Kupfer | 0.1 % Show Supplier Material materials with Kupfer of 0.1 % |
Magnesium | 0.45 - 0.9 % Show Supplier Material materials with Magnesium of 0.45 - 0.9 % |
Mangan | 0.1 % Show Supplier Material materials with Mangan of 0.1 % |
Silizium | 0.2 - 0.6 % Show Supplier Material materials with Silizium of 0.2 - 0.6 % |
Titan | 0.1 % Show Supplier Material materials with Titan of 0.1 % |
Zink | 0.1 % Show Supplier Material materials with Zink of 0.1 % |