Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 25 % Show Supplier Material materials with Dehnung of 25 % |
Dehnung A50 | 23.0 °C | 23 % Show Supplier Material materials with Dehnung A50 of 23 % |
Härte, Brinell | 23.0 °C | 20 [-] Show Supplier Material materials with Härte, Brinell of 20 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 20 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 20 MPa |
Zugfestigkeit | 23.0 °C | 60 MPa Show Supplier Material materials with Zugfestigkeit of 60 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 99.5 % Show Supplier Material materials with Aluminium of 99.5 % |
Andere | 0.03 % Show Supplier Material materials with Andere of 0.03 % |
Eisen | 0.4 % Show Supplier Material materials with Eisen of 0.4 % |
Kupfer | 0.05 % Show Supplier Material materials with Kupfer of 0.05 % |
Magnesium | 0.05 % Show Supplier Material materials with Magnesium of 0.05 % |
Mangan | 0.05 % Show Supplier Material materials with Mangan of 0.05 % |
Silizium | 0.25 % Show Supplier Material materials with Silizium of 0.25 % |
Titan | 0.05 % Show Supplier Material materials with Titan of 0.05 % |
Zink | 0.07 % Show Supplier Material materials with Zink of 0.07 % |
Technological properties
Property | ||
---|---|---|
Coating | suitable for electro-chemical brightening and anodizing | |
Corrosion properties | corrosion resistant | |
Processing methods | Excellent forming properties | |
Welding | weldable |