Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.0032 g/cm³ Show Supplier Material materials with Dichte of 1.0032 g/cm³ | Exact value: 1.00324 |
Mechanisch
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Glasübergangstemperatur | 328 °C Show Supplier Material materials with Glasübergangstemperatur of 328 °C | ||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.8E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.8E-5 1/K | |
Max. Betriebstemperatur | 410 °C Show Supplier Material materials with Max. Betriebstemperatur of 410 °C | decomposition temperature |
Technological properties
Property | ||
---|---|---|
Application areas | High temperature adhesives and bonding |