Allgemein
Property | Value | Comment |
---|---|---|
Contact angle | 91 ° Show Supplier Material materials with Contact angle of 91 ° | with water |
Abmessung
Property | Value | Comment |
---|---|---|
Dicke | 2.5E-4 mm Show Supplier Material materials with Dicke of 2.5E-4 mm | Nominal coat thickness |
Thermisch
Property | Value |
---|---|
Max. Betriebstemperatur | 300 °C Show Supplier Material materials with Max. Betriebstemperatur of 300 °C |
Rheological Properties
Property | Temperature | Value |
---|---|---|
Viskosität | 23.0 °C | 12 Pa·s Show Supplier Material materials with Viskosität of 12 Pa·s |
Technological properties
Property | ||
---|---|---|
Application areas | High temperature temporary adhesives and bonding |