Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.9042 g/cm³ Show Supplier Material materials with Dichte of 0.9042 g/cm³ | Exact value: 0.90424 |
Mechanisch
Property | Temperature | Value |
---|---|---|
Elastizitätsmodul | 23.0 °C | 3.3E-3 GPa Show Supplier Material materials with Elastizitätsmodul of 3.3E-3 GPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Glasübergangstemperatur | -50 °C Show Supplier Material materials with Glasübergangstemperatur of -50 °C | max. | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 3.9E-4 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 3.9E-4 1/K | |
Max. Betriebstemperatur | 350 °C Show Supplier Material materials with Max. Betriebstemperatur of 350 °C | decomposition temperature |
Technological properties
Property | ||
---|---|---|
Application areas | High temperature adhesives and bonding |