Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 1.54 g/cm³ Show Supplier Material materials with Dichte of 1.54 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 20.0 °C | 355 MPa Show Supplier Material materials with Biegefestigkeit of 355 MPa | ISO 178 |
Biegemodul | 20.0 °C | 15.2 GPa Show Supplier Material materials with Biegemodul of 15.2 GPa | ISO 178 |
Dehnung | 20.0 °C | 2.1 % Show Supplier Material materials with Dehnung of 2.1 % | ISO 527-I |
Elastizitätsmodul | 20.0 °C | 17 GPa Show Supplier Material materials with Elastizitätsmodul of 17 GPa | ISO 527-I |
Schlagfestigkeit, Charpy gekerbt | 20.0 °C | 35 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 35 kJ/m² | ISO 179-I |
Zugfestigkeit | 20.0 °C | 240 MPa Show Supplier Material materials with Zugfestigkeit of 240 MPa | ISO 527-I |
Thermisch
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 0.45 MPa | 230 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 230 °C | ISO 75-I |
Technological properties
Property | ||
---|---|---|
Application areas | SKYi Stabil-MH5106 is intended for injection moulding of highly demanding technical applications. The excellent properties of SKYi Stabil-MH5106 make it suitable for: Electrical components, automotive parts, interior, exterior and under the bonnet, structural furniture parts, load bearing, demanding components for various engineering sectors. SKYi Stabil-MH5106 can, in many of these applications, substitute other engineering plastics or metal alloys. | |
Color | Available both in black and natural. Other colours can be provided on request. | |
Other | Safety: SKYi Stabil-MH5106 is not classified as a dangerous preparation. Dust and fines from the product may give a risk for dust explosion. All equipment should be properly earthed. Inhalation of dust may irritate the respiratory system and should be avoided. During processing of the product small amounts of fumes are generated, which require proper ventilation. Recycling: The product is suitable for recycling using modern methods of shredding and cleaning. Inhouse production waste should be kept clean to facilitate direct recycling. A Materials Safety Data Sheet is available on request. Please contact your SKYi representative for more details on various aspects of safety, recovery and disposal of the product. | |
Processing methods | Injection Molding: |