Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 1.63 g/cm³ Show Supplier Material materials with Dichte of 1.63 g/cm³ |
Moisture absorption | 20.0 °C | 0.35 % Show Supplier Material materials with Moisture absorption of 0.35 % |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 20.0 °C | 260 MPa Show Supplier Material materials with Biegefestigkeit of 260 MPa | ISO 178 |
Biegemodul | 20.0 °C | 12 GPa Show Supplier Material materials with Biegemodul of 12 GPa | ISO 178 |
Dehnung | 20.0 °C | 2.3 % Show Supplier Material materials with Dehnung of 2.3 % | ISO 527-I |
Schlagfestigkeit, Charpy gekerbt | 20.0 °C | 15 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 15 kJ/m² | ISO 179-I |
Zugfestigkeit | 20.0 °C | 192 MPa Show Supplier Material materials with Zugfestigkeit of 192 MPa | ISO 527-I |
Thermisch
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 0.45 MPa | 250 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 250 °C | min. ISO 75-I |
Technological properties
Property | ||
---|---|---|
Application areas | SKYi Stark EH2118 is intended for injection moulding of technical applications. The excellent properties of SKYi Stark EH2118 make it suitable for: Electrical components, automotive parts, interior, exterior and under the bonnet, structural furniture parts, load bearing, demanding components for various engineering sectors. SKYi Stark EH2118 can, in many of these applications, substitute other engineering plastics or metal alloys. | |
Color | Available both in black and natural. | |
Other | Safety: SKYi Stark EH2118 is not classified as a dangerous preparation. Dust and fines from the product may give a risk for dust explosion. All equipment should be properly earthed. Inhalation of dust may irritate the respiratory system and should be avoided. During processing of the product small amounts of fumes are generated, which require proper ventilation. Recycling: The product is suitable for recycling using modern methods of shredding and cleaning. Inhouse production waste should be kept clean to facilitate direct recycling. The Materials Safety Data Sheet is available on request. Please contact your SKYi representative for more details on various aspects of safety, recovery and disposal of the product. | |
Processing methods | Injection Molding: |