Allgemein
Property | Temperature | Value | |
---|---|---|---|
Dichte | 23.0 °C | 15.15 g/cm³ Show Supplier Material materials with Dichte of 15.15 g/cm³ | |
Binder | Cobalt binder | ||
Kornstruktur | Fine grain size |
Mechanisch
Property | Temperature | Value |
---|---|---|
Druckfestigkeit | 23.0 °C | 7400 MPa Show Supplier Material materials with Druckfestigkeit of 7400 MPa |
Elastizitätsmodul | 23.0 °C | 650 GPa Show Supplier Material materials with Elastizitätsmodul of 650 GPa |
Härte, Rockwell A | 23.0 °C | 93.1 [-] Show Supplier Material materials with Härte, Rockwell A of 93.1 [-] |
Härte, Vickers, 10 | 23.0 °C | 1845 [-] Show Supplier Material materials with Härte, Vickers, 10 of 1845 [-] |
Plane-Strain Fracture Toughnes | 23.0 °C | 8 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 8 MPa·√m |
Zugfestigkeit, transversal | 23.0 °C | 2050 MPa Show Supplier Material materials with Zugfestigkeit, transversal of 2050 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 4.6E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 4.6E-6 1/K |
Wärmeleitfähigkeit | 23.0 °C | 100 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 100 W/(m·K) |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Kobalt | 4 % Show Supplier Material materials with Kobalt of 4 % | as binder | |
Wolfram | WC balance |
Technological properties
Property |
---|