Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TB00Wrought Copper High Copper Alloy
ASTM B194 Grade C17200 TD04Nickel-Kupfer-Legierung
DIN 17743 Grade NiCu30Fe soft annealed (+A)Kupfer Knetlegierung
CEN/TS 13388 Grade CW112C R300, H070Other Copper Zinc Alloy
EN 1652 Grade CuZn20Al2As R390Kupfer Knetlegierung
CEN/TS 13388 Grade CW109C R240, H050Wrought Copper High Copper Alloy
EN 1652 Grade CuBe2 THWrought Copper Bronze Silicon Bronze
EN 1652 Grade CuNi2Si F00Wrought Copper Bronze Silicon Bronze
EN 1652 Grade CuNi2Si THWrought Copper Bronze Silicon Bronze
EN 1652 Grade CuNi2Si TB00Leaded Brass
EN 12164 Grade CuZn36Pb3 R400Leaded Brass
EN 12164 Grade CuZn36Pb3 R480Other Copper Zinc Alloy
EN 12452 Grade CuZn20Al2As O60Other Copper Zinc Alloy
EN 1652 Grade CuZn20Al2As R330Zinc Aluminium
EN 12844 Grade GD-ZnAl4 cast conditionZinc Aluminium
EN 12844 Grade GD-ZnAl4Cu1 cast condition