Allgemein
Property | Temperature | Value | |
---|---|---|---|
Dichte | 23.0 °C | 14.85 g/cm³ Show Supplier Material materials with Dichte of 14.85 g/cm³ | |
Binder | Cobalt binder | ||
Kornstruktur | Medium grain size |
Mechanisch
Property | Temperature | Value |
---|---|---|
Druckfestigkeit | 23.0 °C | 4800 MPa Show Supplier Material materials with Druckfestigkeit of 4800 MPa |
Elastizitätsmodul | 23.0 °C | 605 GPa Show Supplier Material materials with Elastizitätsmodul of 605 GPa |
Härte, Rockwell A | 23.0 °C | 89.4 [-] Show Supplier Material materials with Härte, Rockwell A of 89.4 [-] |
Härte, Vickers, 10 | 23.0 °C | 1300 [-] Show Supplier Material materials with Härte, Vickers, 10 of 1300 [-] |
Plane-Strain Fracture Toughnes | 23.0 °C | 10.8 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 10.8 MPa·√m |
Zugfestigkeit, transversal | 23.0 °C | 2400 MPa Show Supplier Material materials with Zugfestigkeit, transversal of 2400 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 5.1E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5.1E-6 1/K |
Wärmeleitfähigkeit | 23.0 °C | 100 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 100 W/(m·K) |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Kobalt | 8 % Show Supplier Material materials with Kobalt of 8 % | as binder | |
Wolfram | WC balance |
Technological properties
Property | ||
---|---|---|
Certifications | Compliant with FDA food contact notification number 586 - 591. |