Allgemein
Property | Temperature | Value | |
---|---|---|---|
Dichte | 23.0 °C | 14.65 g/cm³ Show Supplier Material materials with Dichte of 14.65 g/cm³ | |
Binder | Cobalt binder | ||
Kornstruktur | Medium grain size |
Mechanisch
Property | Temperature | Value |
---|---|---|
Druckfestigkeit | 23.0 °C | 5300 MPa Show Supplier Material materials with Druckfestigkeit of 5300 MPa |
Elastizitätsmodul | 23.0 °C | 600 GPa Show Supplier Material materials with Elastizitätsmodul of 600 GPa |
Härte, Rockwell A | 23.0 °C | 90.4 [-] Show Supplier Material materials with Härte, Rockwell A of 90.4 [-] |
Härte, Vickers, 10 | 23.0 °C | 1420 [-] Show Supplier Material materials with Härte, Vickers, 10 of 1420 [-] |
Plane-Strain Fracture Toughnes | 23.0 °C | 11.3 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 11.3 MPa·√m |
Zugfestigkeit, transversal | 23.0 °C | 2800 MPa Show Supplier Material materials with Zugfestigkeit, transversal of 2800 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 5.1E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5.1E-6 1/K |
Wärmeleitfähigkeit | 23.0 °C | 95 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 95 W/(m·K) |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Kobalt | 8.5 % Show Supplier Material materials with Kobalt of 8.5 % | as binder | |
Wolfram | WC balance |
Technological properties