Allgemein
Property | Temperature | Value | |
---|---|---|---|
Dichte | 23.0 °C | 15.2 g/cm³ Show Supplier Material materials with Dichte of 15.2 g/cm³ | |
Binder | Cobalt binder | ||
Kornstruktur | Submicron grain size |
Mechanisch
Property | Temperature | Value |
---|---|---|
Druckfestigkeit | 23.0 °C | 10100 MPa Show Supplier Material materials with Druckfestigkeit of 10100 MPa |
Elastizitätsmodul | 23.0 °C | 655 GPa Show Supplier Material materials with Elastizitätsmodul of 655 GPa |
Härte, Rockwell A | 23.0 °C | 93.4 [-] Show Supplier Material materials with Härte, Rockwell A of 93.4 [-] |
Härte, Vickers, 10 | 23.0 °C | 1920 [-] Show Supplier Material materials with Härte, Vickers, 10 of 1920 [-] |
Plane-Strain Fracture Toughnes | 23.0 °C | 8.7 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 8.7 MPa·√m |
Zugfestigkeit, transversal | 23.0 °C | 2300 MPa Show Supplier Material materials with Zugfestigkeit, transversal of 2300 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 4.6E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 4.6E-6 1/K |
Wärmeleitfähigkeit | 23.0 °C | 90 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 90 W/(m·K) |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Kobalt | 4.2 % Show Supplier Material materials with Kobalt of 4.2 % | as binder | |
Wolfram | WC balance |
Technological properties
Property |
---|