Description

2.0855 (CuNi2Si) is a precipitation hardening copper nickel silicon that offers a remarkable blend of physical and mechanical attributes unrivalled by many other grades of copper alloy. Colsibro® is a high copper alloy with small additions of nickel and silicon, which combine to increase the strength, hardness and wear resistance of the material, while retaining many of the physical benefits of copper itself. It shows the following features and properties:


  • Excellent corrosion resistance, surpassing many copper alloys, with complete freedom from stress corrosion
  • High strength and hardness
  • Very good wear resistance and bearing properties
  • Excellent thermal and electrical conductivities compared to most non-ferrous alloys
  • Outstanding cryogenic properties and an exceptionally low magnetic permeability
  • Complete freedom from hydrogen embrittlement
  • Spark resistance
  • Related Standards

    Equivalent Materials

    Diese Materialdaten wurden von Matmatch zur Verfügung gestellt

    Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
    Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

    Ashby charts

    Eigenschaften

    Allgemein

    PropertyTemperatureValue

    Dichte

    23.0 °C

    8.87 g/cm³

    Show Material materials with Dichte of 8.87 g/cm³

    Mechanisch

    PropertyTemperatureValue

    Dehnung

    23.0 °C

    10 %

    Show Material materials with Dehnung of 10 %

    Härte, Brinell

    23.0 °C

    155 - 180 [-]

    Show Material materials with Härte, Brinell of 155 - 180 [-]

    Streckgrenze Rp 0,2

    23.0 °C

    430 - 590 MPa

    Show Material materials with Streckgrenze Rp 0,2 of 430 - 590 MPa

    Zugfestigkeit

    23.0 °C

    550 - 640 MPa

    Show Material materials with Zugfestigkeit of 550 - 640 MPa

    Thermisch

    PropertyTemperatureValueComment

    Koeffizient der thermischen Ausdehnung

    23.0 °C

    1.6E-5 1/K

    Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 1/K

    for 0-400°C

    Schmelzpunkt

    1040 - 1060 °C

    Show Material materials with Schmelzpunkt of 1040 - 1060 °C

    Wärmeleitfähigkeit

    23.0 °C

    160 W/(m·K)

    Show Material materials with Wärmeleitfähigkeit of 160 W/(m·K)

    Elektrisch

    PropertyTemperatureValue

    Elektrische Leitfähigkeit

    23.0 °C

    2.03E+7 S/m

    Show Material materials with Elektrische Leitfähigkeit of 2.03E+7 S/m

    Specific Electrical conductivity

    35 % IACS

    Show Material materials with Specific Electrical conductivity of 35 % IACS

    Magnetisch

    PropertyTemperatureValue

    Relative magnetische Permeabilität

    23.0 °C

    1 [-]

    Show Material materials with Relative magnetische Permeabilität of 1 [-]

    Chemical properties

    PropertyValue

    Kupfer

    Balance

    Nickel

    1.6 - 2.2 %

    Show Material materials with Nickel of 1.6 - 2.2 %

    Silizium

    0.4 - 0.8 %

    Show Material materials with Silizium of 0.4 - 0.8 %

    Technological properties

    Property
    Application areas

    Automotive: Valve guides, valve seats, gears, rocker and little end bushes or internal combustion engines requiring extreme performance;Offshore & marine: Fasteners, valves, choke stems, down-hole tooling, cryogenic storage tanks and pump bodies;Electrical: current-carrying electrical components such as slip rings, squirrel cages, springs, rotary switch contacts, contact blades, short-circuit rings and heavy duty switchgear;Other: Non-magnetic instrument components and spark-resistant safety tooling

    Cold Forming

    It can be cold formed

    Corrosion properties

    Excellent corrosion resistance

    General machinability

    Easily machined

    Hot forming

    It can be hot formed