1.4542 (X5CrNiCuNb16-4) is a well-established precipitation hardening martensitic stainless steel capable of achieving very high strength and hardness after a relatively simple heat treatment. It offers excellent corrosion resistance combined with a structured range of mechanical property levels depending on the precise heat treatment applied. It is readily machined and fabricated in the softer tempers and can then be heat-treated to exceptional strength and dimensional stability. It shows the following features and properties:


  • Very high strength
  • Very good resistance to pitting and crevice corrosion
  • Excellent resistance to chloride stress corrosion cracking
  • Good workability and weldability
  • Related Standards

    Equivalent Materials

    Diese Materialdaten wurden von Matmatch zur Verfügung gestellt

    Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
    Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

    Ashby charts

    Eigenschaften

    Chemical properties

    PropertyValueComment

    Chrom

    17 %

    Show Material materials with Chrom of 17 %

    Eisen

    Balance

    Kupfer

    4 %

    Show Material materials with Kupfer of 4 %

    Nickel

    4 %

    Show Material materials with Nickel of 4 %

    Niobium

    0.3 %

    Show Material materials with Niobium of 0.3 %

    Nb+Ta

    Tantal

    0.3 %

    Show Material materials with Tantal of 0.3 %

    Nb+Ta

    Technological properties

    Property
    Application areas

    Offshore & marine: Offshore foils, helicopter deck platforms, pump shafts, couplings, fasteners, valve parts and spindles;Aerospace: Turbine blades, missile and rocket fittings, undercarriage components and fasteners;Other: Nuclear waste casks, medical instruments, paper mill equipment and chemical process plant, springs, screws, bolts, gears, bushes and wear rings

    Corrosion properties

    Very high corrosion resistance

    General machinability

    It is readily machinable