Formadur 2083 Superclean Plate

Alternative und Handelsbezeichungen
DIN EN ISO X40Cr14, AISI 420, 1.2083, AFNOR Z40C14
Want to keep this datasheet? Save it now in your required format

Beschreibung

1.2083 (X40Cr14) Quenched and Tempered steel plate exhibits good corrosion-resistant and excellent polishability.

Equivalent Materials

Eigenschaften

Abmessung

Thickness

t

40 - 350 mm

Width

w

900 - 1100 mm

Mechanisch

Hardness, Brinell

HB

230 [-] at 20 °C

soft annealed

Hardness, Rockwell C

HRC

48 - 56 [-] at 20 °C

Tensile strength

Rm

1555 - 1775 MPa at 20 °C

Thermisch

Coefficient of thermal expansion

α

1.11E-5 1/K at 100 °C

for 20°C to the mentioned temperature

Grafik verstecken

Thermal conductivity

λ

22.6 W/(m·K) at 23 °C

Unlock all property charts

Create your account on Matmatch to view all property charts and access other premium features for free.

Anmelden

Chemische Eigenschaften

Element

Gew. %

Kommentar

Fe

-

Balance

Cr

13.5 %

Mn

0.9 %

C

0.4 %

Si

0.35 %

Technische Eigenschaften

Application areas

Moulds and inserts for processing corrosive acting plastics.

Heat Treatment

Soft annealing: 760-800°C (Cooling in furnace) - Hardening: 1000-1050°C and quenching in air, oil or hot bath T=500-550°C

Do you need more data regarding this material?

Diese Materialdaten wurden von Deutsche Edelstahlwerke Specialty Steel (DEW) zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.