Abmessung
Property | Value |
---|---|
Breite | 900 - 1100 mm Show Supplier Material materials with Breite of 900 - 1100 mm |
Dicke | 200 - 500 mm Show Supplier Material materials with Dicke of 200 - 500 mm |
Mechanisch
Property | Value |
---|---|
Härte, Rockwell C | 38 - 42 [-] Show Supplier Material materials with Härte, Rockwell C of 38 - 42 [-] |
Zugfestigkeit | 1190 - 1320 MPa Show Supplier Material materials with Zugfestigkeit of 1190 - 1320 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100 °C | 1.04e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.04e-05 1/K | for 20°C to the mentioned temperature |
150 °C | 1.06e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.06e-05 1/K | for 20°C to the mentioned temperature | |
200 °C | 1.09e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.09e-05 1/K | for 20°C to the mentioned temperature | |
250 °C | 1.11e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.11e-05 1/K | for 20°C to the mentioned temperature | |
300 °C | 1.14e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.14e-05 1/K | for 20°C to the mentioned temperature | |
350 °C | 1.15e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.15e-05 1/K | for 20°C to the mentioned temperature | |
400 °C | 1.17e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.17e-05 1/K | for 20°C to the mentioned temperature | |
450 °C | 1.19e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.19e-05 1/K | for 20°C to the mentioned temperature | |
500 °C | 1.2e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.2e-05 1/K | for 20°C to the mentioned temperature | |
Wärmeleitfähigkeit | 23 °C | 16.8 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 16.8 W/(m·K) | |
150 °C | 20.1 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 20.1 W/(m·K) | ||
300 °C | 22.1 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 22.1 W/(m·K) | ||
350 °C | 22.8 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 22.8 W/(m·K) | ||
400 °C | 23.3 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 23.3 W/(m·K) | ||
500 °C | 24.1 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 24.1 W/(m·K) |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Andere | 3.5 % Show Supplier Material materials with Andere of 3.5 % | Cu + Nb | |
Chrom | 15 % Show Supplier Material materials with Chrom of 15 % | ||
Eisen | Balance | ||
Kohlenstoff | 0.05 % Show Supplier Material materials with Kohlenstoff of 0.05 % | ||
Mangan | 0.3 % Show Supplier Material materials with Mangan of 0.3 % | ||
Nickel | 4.5 % Show Supplier Material materials with Nickel of 4.5 % | ||
Silizium | 0.3 % Show Supplier Material materials with Silizium of 0.3 % |
Technological properties
Property | ||
---|---|---|
Application areas | High polished tools and moulds for processing of high corrosive plastics, tools for plastic extrusion. | |
Heat Treatment | Formadur PH X Superclean usually is supplied in precipitation-hardened condition with a hardness of 40 HRC. |