Abmessung
Property | Value |
---|---|
Breite | 700 - 1010 mm Show Supplier Material materials with Breite of 700 - 1010 mm |
Dicke | 15 - 225 mm Show Supplier Material materials with Dicke of 15 - 225 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Härte, Brinell | 280 - 325 [-] Show Supplier Material materials with Härte, Brinell of 280 - 325 [-] | as-delivered condition |
Härte, Rockwell C | 30 - 48 [-] Show Supplier Material materials with Härte, Rockwell C of 30 - 48 [-] | |
Zugfestigkeit | 950 - 1095 MPa Show Supplier Material materials with Zugfestigkeit of 950 - 1095 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 16 % Show Supplier Material materials with Chrom of 16 % |
Eisen | Balance |
Kohlenstoff | 0.33 % Show Supplier Material materials with Kohlenstoff of 0.33 % |
Mangan | 1.2 % Show Supplier Material materials with Mangan of 1.2 % |
Nickel | 0.5 % Show Supplier Material materials with Nickel of 0.5 % |
Schwefel | 0.05 % Show Supplier Material materials with Schwefel of 0.05 % |
Silizium | 0.3 % Show Supplier Material materials with Silizium of 0.3 % |
Technological properties
Property | ||
---|---|---|
Application areas | Mould frames, plastic moulds without special demands on surface quality. | |
Heat Treatment | Soft annealing: 850-880°C (Cooling in furnace) - Hardening: 1000-1050°C and quenching in oil |