Allgemein
Property | Value |
---|---|
Dichte | 7.7 g/cm³ Show Supplier Material materials with Dichte of 7.7 g/cm³ |
Abmessung
Property | Value |
---|---|
Breite | 1050 - 1250 mm Show Supplier Material materials with Breite of 1050 - 1250 mm |
Dicke | 40 - 220 mm Show Supplier Material materials with Dicke of 40 - 220 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 13 % Show Supplier Material materials with Dehnung of 13 % | ||
Elastizitätsmodul | 20 °C | 214.6 GPa Show Supplier Material materials with Elastizitätsmodul of 214.6 GPa | |
Flächenreduzierung | 42 % Show Supplier Material materials with Flächenreduzierung of 42 % | ||
Härte, Brinell | 280 - 325 [-] Show Supplier Material materials with Härte, Brinell of 280 - 325 [-] | as-delivered condition | |
Streckgrenze | 890 MPa Show Supplier Material materials with Streckgrenze of 890 MPa | RP02 | |
Zugfestigkeit | 950 - 1100 MPa Show Supplier Material materials with Zugfestigkeit of 950 - 1100 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100 °C | 1.03e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.03e-05 1/K | for 20°C to the mentioned temperature |
150 °C | 1.06e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.06e-05 1/K | for 20°C to the mentioned temperature | |
200 °C | 1.09e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.09e-05 1/K | for 20°C to the mentioned temperature | |
250 °C | 1.11e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.11e-05 1/K | for 20°C to the mentioned temperature | |
300 °C | 1.12e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.12e-05 1/K | for 20°C to the mentioned temperature | |
350 °C | 1.14e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.14e-05 1/K | for 20°C to the mentioned temperature | |
400 °C | 1.16e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.16e-05 1/K | for 20°C to the mentioned temperature | |
450 °C | 1.18e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.18e-05 1/K | for 20°C to the mentioned temperature | |
500 °C | 1.2e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.2e-05 1/K | for 20°C to the mentioned temperature | |
Wärmeleitfähigkeit | 23 °C | 24.6 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 24.6 W/(m·K) | |
150 °C | 25.7 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 25.7 W/(m·K) | ||
300 °C | 25.8 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 25.8 W/(m·K) | ||
350 °C | 25.7 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 25.7 W/(m·K) | ||
400 °C | 25.4 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 25.4 W/(m·K) | ||
500 °C | 24.7 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 24.7 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Andere | Plus additions |
Chrom | 12.5 % Show Supplier Material materials with Chrom of 12.5 % |
Eisen | Balance |
Kohlenstoff | 0.05 % Show Supplier Material materials with Kohlenstoff of 0.05 % |
Mangan | 1.3 % Show Supplier Material materials with Mangan of 1.3 % |
Schwefel | 0.15 % Show Supplier Material materials with Schwefel of 0.15 % |
Silizium | 0.4 % Show Supplier Material materials with Silizium of 0.4 % |
Technological properties
Property | ||
---|---|---|
Application areas | Base plates, mould bases and plastic moulds without special requirements on polishability, as well as being resistant to condensation and cooling water (All-Stainless-Concept) |