Allgemein
Property | Value |
---|---|
Dichte | 7.6 g/cm³ Show Supplier Material materials with Dichte of 7.6 g/cm³ |
Mechanisch
Property | Value | Comment |
---|---|---|
Härte, Brinell | 270 - 315 [-] Show Supplier Material materials with Härte, Brinell of 270 - 315 [-] | as-delivered condition |
Zugfestigkeit | 915 - 1060 MPa Show Supplier Material materials with Zugfestigkeit of 915 - 1060 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100 °C | 8.5e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 8.5e-06 1/K | for 20°C to the mentioned temperature |
200 °C | 1e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1e-05 1/K | for 20°C to the mentioned temperature | |
300 °C | 1.52e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.52e-05 1/K | for 20°C to the mentioned temperature | |
400 °C | 1.46e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.46e-05 1/K | for 20°C to the mentioned temperature | |
500 °C | 1.43e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.43e-05 1/K | for 20°C to the mentioned temperature | |
Wärmeleitfähigkeit | 23 °C | 22.2 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 22.2 W/(m·K) | |
150 °C | 22.6 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 22.6 W/(m·K) | ||
350 °C | 23.2 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 23.2 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Andere | Plus additions |
Chrom | 12.8 % Show Supplier Material materials with Chrom of 12.8 % |
Eisen | Balance |
Kohlenstoff | 0.22 % Show Supplier Material materials with Kohlenstoff of 0.22 % |
Mangan | 1.6 % Show Supplier Material materials with Mangan of 1.6 % |
Schwefel | 0.12 % Show Supplier Material materials with Schwefel of 0.12 % |
Silizium | 0.25 % Show Supplier Material materials with Silizium of 0.25 % |
Technological properties
Property | ||
---|---|---|
Application areas | Complex base plates and mould frames with highest demands on machinability and resistance to condensation and cooling water (All-Stainless-Concept), plastic moulds without special requirements on polishability. | |
Corrosion properties | Consistent corrosion resistance: Even when additional corrosion resistance materials are used, which combined with other steels would have triggered contact corrosion | |
General machinability | Good stability despite time-consuming machining of the raw material: Even for filigree componenets and limited cavity spacing. |