Abmessung
Property | Value |
---|---|
Durchmesser | 26 - 252 mm Show Supplier Material materials with Durchmesser of 26 - 252 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Härte, Brinell | 230 [-] Show Supplier Material materials with Härte, Brinell of 230 [-] | soft annealed |
Härte, Rockwell C | 42 - 52 [-] Show Supplier Material materials with Härte, Rockwell C of 42 - 52 [-] | |
Zugfestigkeit | 1320 - 1775 MPa Show Supplier Material materials with Zugfestigkeit of 1320 - 1775 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100 °C | 1.13e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.13e-05 1/K | for 20°C to the mentioned temperature |
200 °C | 1.19e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.19e-05 1/K | for 20°C to the mentioned temperature | |
300 °C | 1.22e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.22e-05 1/K | for 20°C to the mentioned temperature | |
400 °C | 1.26e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.26e-05 1/K | for 20°C to the mentioned temperature | |
500 °C | 1.3e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.3e-05 1/K | for 20°C to the mentioned temperature | |
600 °C | 1.33e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.33e-05 1/K | for 20°C to the mentioned temperature | |
700 °C | 1.35e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.35e-05 1/K | for 20°C to the mentioned temperature | |
Wärmeleitfähigkeit | 20 °C | 31.4 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 31.4 W/(m·K) | |
350 °C | 35.2 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 35.2 W/(m·K) | ||
700 °C | 36.2 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 36.2 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Chrom | 3 % Show Supplier Material materials with Chrom of 3 % |
Eisen | Balance |
Kohlenstoff | 0.45 % Show Supplier Material materials with Kohlenstoff of 0.45 % |
Mangan | 0.3 % Show Supplier Material materials with Mangan of 0.3 % |
Silizium | 0.3 % Show Supplier Material materials with Silizium of 0.3 % |
Vanadium | 1 % Show Supplier Material materials with Vanadium of 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | For use at highest temperatures, highly wear-exposed die inserts, high speed forging machines, casting dies for heavy metal processing | |
Heat Treatment | Soft annealing: 750-800°C (Cooling in furnace) - Hardening: 1070-1100°C and quenching in air, oil or hot bath T=500-550°C |