Abmessung
Property | Value |
---|---|
Durchmesser | 232 - 363 mm Show Supplier Material materials with Durchmesser of 232 - 363 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Härte, Brinell | 230 [-] Show Supplier Material materials with Härte, Brinell of 230 [-] | soft annealed |
Härte, Rockwell C | 42 - 52 [-] Show Supplier Material materials with Härte, Rockwell C of 42 - 52 [-] | |
Zugfestigkeit | 1320 - 1775 MPa Show Supplier Material materials with Zugfestigkeit of 1320 - 1775 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100 °C | 1.15e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.15e-05 1/K | for 20°C to the mentioned temperature |
200 °C | 1.2e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.2e-05 1/K | for 20°C to the mentioned temperature | |
300 °C | 1.23e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.23e-05 1/K | for 20°C to the mentioned temperature | |
400 °C | 1.26e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.26e-05 1/K | for 20°C to the mentioned temperature | |
500 °C | 1.29e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.29e-05 1/K | for 20°C to the mentioned temperature | |
600 °C | 1.32e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.32e-05 1/K | for 20°C to the mentioned temperature | |
Wärmeleitfähigkeit | 20 °C | 28.36 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 28.36 W/(m·K) | |
100 °C | 29.3 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 29.3 W/(m·K) | ||
200 °C | 30.9 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 30.9 W/(m·K) | ||
300 °C | 31 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 31 W/(m·K) | ||
400 °C | 30.7 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 30.7 W/(m·K) | ||
500 °C | 29.5 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 29.5 W/(m·K) | ||
600 °C | 27.8 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 27.8 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Andere | Plus additions |
Chrom | 5 % Show Supplier Material materials with Chrom of 5 % |
Eisen | Balance |
Kohlenstoff | 0.35 % Show Supplier Material materials with Kohlenstoff of 0.35 % |
Mangan | 0.3 % Show Supplier Material materials with Mangan of 0.3 % |
Silizium | 0.3 % Show Supplier Material materials with Silizium of 0.3 % |
Vanadium | 0.8 % Show Supplier Material materials with Vanadium of 0.8 % |
Technological properties
Property | ||
---|---|---|
Application areas | Universally usable for highly stressed tools and highest temperatures, casting dies for light metal processing (especially for complex tools), extrusion dies for light and heavy metal processing (especially for complexly formed profiles), dies and inserts | |
Heat Treatment | Soft annealing: 750-800°C (Cooling in furnace) - Hardening: 1020-1040°C and quenching in air, oil or hot bath T=500-550°C |