Abmessung
Property | Value |
---|---|
Breite | 1030 mm Show Supplier Material materials with Breite of 1030 mm |
Dicke | 25 - 130 mm Show Supplier Material materials with Dicke of 25 - 130 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Härte, Brinell | 231 [-] Show Supplier Material materials with Härte, Brinell of 231 [-] | soft annealed |
Härte, Rockwell C | 56 - 62 [-] Show Supplier Material materials with Härte, Rockwell C of 56 - 62 [-] |
Thermisch
Property | Temperature | Value |
---|---|---|
Wärmeleitfähigkeit | 100 °C | 15.8 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 15.8 W/(m·K) |
350 °C | 26.7 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 26.7 W/(m·K) | |
700 °C | 29.1 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 29.1 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Chrom | 5 % Show Supplier Material materials with Chrom of 5 % |
Eisen | Balance |
Kohlenstoff | 1 % Show Supplier Material materials with Kohlenstoff of 1 % |
Mangan | 0.5 % Show Supplier Material materials with Mangan of 0.5 % |
Molybdän | 0.95 % Show Supplier Material materials with Molybdän of 0.95 % |
Silizium | 0.3 % Show Supplier Material materials with Silizium of 0.3 % |
Vanadium | 0.2 % Show Supplier Material materials with Vanadium of 0.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Cutting tools, rolls, shear blades, cold pilger mandrels, cold stamping tools, plastic moulds | |
Heat Treatment | Soft annealing: 610-650°C (Cooling in furnace) - Stress-relief-annealing: 600°C (cooling in Furnace), Hardening: 930-970°C and quenching in oil, air or salt bath: 500-550°C |