Abmessung
Property | Value |
---|---|
Breite | 1010 mm Show Supplier Material materials with Breite of 1010 mm |
Dicke | 20 - 80 mm Show Supplier Material materials with Dicke of 20 - 80 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Härte, Brinell | 230 [-] Show Supplier Material materials with Härte, Brinell of 230 [-] | soft annealed |
Härte, Rockwell C | 54 - 61 [-] Show Supplier Material materials with Härte, Rockwell C of 54 - 61 [-] |
Thermisch
Property | Temperature | Value |
---|---|---|
Wärmeleitfähigkeit | 20 °C | 33.5 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 33.5 W/(m·K) |
350 °C | 32 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 32 W/(m·K) | |
700 °C | 30.9 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 30.9 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Chrom | 0.6 % Show Supplier Material materials with Chrom of 0.6 % |
Eisen | Balance |
Kohlenstoff | 0.95 % Show Supplier Material materials with Kohlenstoff of 0.95 % |
Mangan | 1.1 % Show Supplier Material materials with Mangan of 1.1 % |
Silizium | 0.2 % Show Supplier Material materials with Silizium of 0.2 % |
Vanadium | 0.1 % Show Supplier Material materials with Vanadium of 0.1 % |
Wolfram | 0.6 % Show Supplier Material materials with Wolfram of 0.6 % |
Technological properties
Property | ||
---|---|---|
Application areas | Blanking and stamping dies for cutting sheets, threading tools, drills, broaches, gauges, measuring tools, plastic moulds, shear blades, guide rails | |
Heat Treatment | Soft annealing: 740-770°C (Cooling in furnace) - Stress-relief-annealing: 650°C (cooling in Furnace), Hardening: 780-820°C and quenching in oil or salt bath: 180-220°C |