Abmessung
Property | Value |
---|---|
Durchmesser | 20 - 122 mm Show Supplier Material materials with Durchmesser of 20 - 122 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Härte, Brinell | 225 [-] Show Supplier Material materials with Härte, Brinell of 225 [-] | soft annealed |
Härte, Rockwell C | 54 - 58 [-] Show Supplier Material materials with Härte, Rockwell C of 54 - 58 [-] | |
Zugfestigkeit | 1920 - 2180 MPa Show Supplier Material materials with Zugfestigkeit of 1920 - 2180 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100 °C | 1.18e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.18e-05 1/K | for 20°C to the mentioned temperature |
200 °C | 1.27e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.27e-05 1/K | for 20°C to the mentioned temperature | |
300 °C | 1.31e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.31e-05 1/K | for 20°C to the mentioned temperature | |
400 °C | 1.35e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.35e-05 1/K | for 20°C to the mentioned temperature | |
500 °C | 1.4e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.4e-05 1/K | for 20°C to the mentioned temperature | |
600 °C | 1.43e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.43e-05 1/K | for 20°C to the mentioned temperature | |
700 °C | 1.45e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.45e-05 1/K | for 20°C to the mentioned temperature | |
Wärmeleitfähigkeit | 20 °C | 34.2 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 34.2 W/(m·K) | |
350 °C | 32.6 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 32.6 W/(m·K) | ||
700 °C | 30.9 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 30.9 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Chrom | 1.1 % Show Supplier Material materials with Chrom of 1.1 % |
Eisen | Balance |
Kohlenstoff | 0.6 % Show Supplier Material materials with Kohlenstoff of 0.6 % |
Mangan | 0.35 % Show Supplier Material materials with Mangan of 0.35 % |
Silizium | 0.6 % Show Supplier Material materials with Silizium of 0.6 % |
Vanadium | 0.2 % Show Supplier Material materials with Vanadium of 0.2 % |
Wolfram | 2 % Show Supplier Material materials with Wolfram of 2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Blanking dies for cutting sheets, trimming and splitting dies, cold piercing punches, tableting tools, shear blades, chopping knives, pneumatic chisels, coining tools, cold shear blades, ejectors | |
Heat Treatment | Soft annealing: 710-750°C (Cooling in furnace) - Stress-relief-annealing: 650°C (cooling in Furnace), Hardening: 870-900°C and quenching in oil or salt bath: 500-550°C |