Mechanisch
Property | Value | Comment |
---|---|---|
Härte, Brinell | 295 [-] Show Supplier Material materials with Härte, Brinell of 295 [-] | soft annealed |
Härte, Rockwell C | 50 - 54 [-] Show Supplier Material materials with Härte, Rockwell C of 50 - 54 [-] | |
Zugfestigkeit | 1665 - 1920 MPa Show Supplier Material materials with Zugfestigkeit of 1665 - 1920 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 1.5 % Show Supplier Material materials with Chrom of 1.5 % |
Eisen | Balance |
Kohlenstoff | 0.45 % Show Supplier Material materials with Kohlenstoff of 0.45 % |
Mangan | 0.7 % Show Supplier Material materials with Mangan of 0.7 % |
Molybdän | 0.8 % Show Supplier Material materials with Molybdän of 0.8 % |
Nickel | 4 % Show Supplier Material materials with Nickel of 4 % |
Silizium | 0.25 % Show Supplier Material materials with Silizium of 0.25 % |
Vanadium | 0.5 % Show Supplier Material materials with Vanadium of 0.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Special steel for cold-shear blades, particularly for cutting scrap, drawing jaws, coining and bending tools | |
Heat Treatment | Soft annealing: 610-650°C (Cooling in furnace) - Stress-relief-annealing: 600°C (cooling in Furnace), Hardening: 880-910°C and quenching in air, oil or salt bath: 180-220°C |