Abmessung
Property | Value |
---|---|
Durchmesser | 10 - 220 mm Show Supplier Material materials with Durchmesser of 10 - 220 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Härte, Brinell | 220 [-] Show Supplier Material materials with Härte, Brinell of 220 [-] | soft annealed |
Härte, Rockwell C | 51 - 59 [-] Show Supplier Material materials with Härte, Rockwell C of 51 - 59 [-] |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Special steel for spring collets | |
Heat Treatment | Soft annealing: 680-720°C (Cooling in furnace) - Stress-relief-annealing: 650°C (cooling in Furnace), Hardening: 820-860°C and quenching in air, oil or salt bath: 180-220°C |