Show me around

Cryodur 2842 Plate

Alternative und Handelsbezeichungen
DIN EN ISO 90MnCrV8, 1.2842, AISI O2
Want to keep this datasheet? Save it now in your required format

Beschreibung

1.2842 (90MnCrV8) Quenched and Tempered steel plate with good cutting edge retention, dimensionally stable during heat treatment.

Equivalent Materials

Eigenschaften

Abmessung

Thickness

t

15 - 200 mm

Width

w

1010 mm

Mechanisch

Hardness, Brinell

HB

220 [-] at 20 °C

soft annealed

Hardness, Rockwell C

HRC

56 - 60 [-] at 20 °C

Thermisch

Coefficient of thermal expansion

α

1.22E-5 1/K at 100 °C

for 20°C to the mentioned temperature

Grafik verstecken

Thermal conductivity

λ

33 W/(m·K) at 20 °C

Unlock all property charts

Create your account on Matmatch to view all property charts and access other premium features for free.

Anmelden

Chemische Eigenschaften

Element

Gew. %

Kommentar

Fe

-

Balance

Mn

2 %

C

0.9 %

Cr

0.4 %

Si

0.2 %

Mehr

Technische Eigenschaften

Application areas

Universally usable, cutting and stamping tools, thread-cutting tools, reamers, gauges, measuring tools, plastic moulds, shear blades, guide rails, ejector pins

Heat Treatment

Soft annealing: 680-720°C (Cooling in furnace) - Stress-relief-annealing: 650°C (cooling in Furnace), Hardening: 790-820°C and quenching in air, oil or salt bath: 180-220°C

Do you need more data regarding this material?

Diese Materialdaten wurden von Deutsche Edelstahlwerke Specialty Steel (DEW) zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.