Mechanisch
Property | Value | Comment |
---|---|---|
Härte, Brinell | 302 [-] Show Supplier Material materials with Härte, Brinell of 302 [-] | annealed |
Härte, Rockwell C | 65 - 67 [-] Show Supplier Material materials with Härte, Rockwell C of 65 - 67 [-] |
Chemical properties
Property | Value |
---|---|
Chrom | 4.1 % Show Supplier Material materials with Chrom of 4.1 % |
Eisen | Balance |
Kobalt | 10 % Show Supplier Material materials with Kobalt of 10 % |
Kohlenstoff | 1.23 % Show Supplier Material materials with Kohlenstoff of 1.23 % |
Molybdän | 3.5 % Show Supplier Material materials with Molybdän of 3.5 % |
Vanadium | 3.3 % Show Supplier Material materials with Vanadium of 3.3 % |
Wolfram | 9.5 % Show Supplier Material materials with Wolfram of 9.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Universally applicable for roughing and for automatic lathes and in generall all kinds of cutting tools and milling cutters. | |
Heat Treatment | Soft annealing: 820-860°C (Cooling in furnace) - Stress relief annealing: 630-650°C (Cooling in furnace) - Hardening: 1190-1230°C and quenching in air, oil or salt bath T=500-550°C - Tempering: at least 3 times 540-570°C |