Mechanisch
Property | Value | Comment |
---|---|---|
Härte, Brinell | 269 [-] Show Supplier Material materials with Härte, Brinell of 269 [-] | annealed |
Härte, Rockwell C | 64 - 67 [-] Show Supplier Material materials with Härte, Rockwell C of 64 - 67 [-] |
Chemical properties
Property | Value |
---|---|
Chrom | 4.1 % Show Supplier Material materials with Chrom of 4.1 % |
Eisen | Balance |
Kobalt | 4.8 % Show Supplier Material materials with Kobalt of 4.8 % |
Kohlenstoff | 0.92 % Show Supplier Material materials with Kohlenstoff of 0.92 % |
Molybdän | 5 % Show Supplier Material materials with Molybdän of 5 % |
Vanadium | 1.9 % Show Supplier Material materials with Vanadium of 1.9 % |
Wolfram | 6.4 % Show Supplier Material materials with Wolfram of 6.4 % |
Technological properties
Property | ||
---|---|---|
Application areas | Heavy-duty milling cutters, highly stressed twist drills and taps, profile knives, machining of high-strength materials, broaches | |
Heat Treatment | Soft annealing: 820-860°C (Cooling in furnace) - Stress relief annealing: 630-650°C (Cooling in furnace) - Hardening: 1190-1230°C and quenching in air, oil or salt bath T=550°C - Tempering: at least 3 times 540-570°C |