Abmessung
Property | Value |
---|---|
Durchmesser | 10 - 323 mm Show Supplier Material materials with Durchmesser of 10 - 323 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Härte, Brinell | 269 [-] Show Supplier Material materials with Härte, Brinell of 269 [-] | annealed |
Härte, Rockwell C | 64 - 66 [-] Show Supplier Material materials with Härte, Rockwell C of 64 - 66 [-] |
Thermisch
Property | Temperature | Value |
---|---|---|
Wärmeleitfähigkeit | 20 °C | 32.8 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 32.8 W/(m·K) |
350 °C | 23.5 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 23.5 W/(m·K) | |
700 °C | 25.5 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 25.5 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Chrom | 4.1 % Show Supplier Material materials with Chrom of 4.1 % |
Eisen | Balance |
Kohlenstoff | 0.9 % Show Supplier Material materials with Kohlenstoff of 0.9 % |
Molybdän | 5 % Show Supplier Material materials with Molybdän of 5 % |
Vanadium | 1.9 % Show Supplier Material materials with Vanadium of 1.9 % |
Wolfram | 6.4 % Show Supplier Material materials with Wolfram of 6.4 % |
Technological properties
Property | ||
---|---|---|
Application areas | Metal-cutting tools for roughing or finishing, shaping tools, woodworking tools, suitable for cold-forming tools | |
Heat Treatment | Soft annealing: 820-860°C (Cooling in furnace) - Stress relief annealing: 630-650°C (Cooling in furnace) - Hardening: 1190-1230°C and quenching in air, oil or salt bath T=530-560°C - Tempering: at least 3 times 530-560°C |