Allgemein
Property | Value |
---|---|
Dichte | 7.4 g/cm³ Show Supplier Material materials with Dichte of 7.4 g/cm³ |
Mechanisch
Property | Value |
---|---|
Elastizitätsmodul | 220 GPa Show Supplier Material materials with Elastizitätsmodul of 220 GPa |
Härte, Rockwell C | 59 - 62 [-] Show Supplier Material materials with Härte, Rockwell C of 59 - 62 [-] |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100 °C | 1.1e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.1e-05 1/K | for 20°C to the mentioned temperature |
200 °C | 1.11e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.11e-05 1/K | for 20°C to the mentioned temperature | |
300 °C | 1.13e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.13e-05 1/K | for 20°C to the mentioned temperature | |
400 °C | 1.15e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.15e-05 1/K | for 20°C to the mentioned temperature |
Chemical properties
Property | Value |
---|---|
Chrom | 5.3 % Show Supplier Material materials with Chrom of 5.3 % |
Eisen | Balance |
Kohlenstoff | 2.45 % Show Supplier Material materials with Kohlenstoff of 2.45 % |
Mangan | 0.5 % Show Supplier Material materials with Mangan of 0.5 % |
Molybdän | 1.3 % Show Supplier Material materials with Molybdän of 1.3 % |
Schwefel | 0.05 % Show Supplier Material materials with Schwefel of 0.05 % |
Silizium | 0.9 % Show Supplier Material materials with Silizium of 0.9 % |
Vanadium | 10 % Show Supplier Material materials with Vanadium of 10 % |
Technological properties
Property | ||
---|---|---|
Application areas | Various applications for cold work: punches, bending dies, cold forming presses, cutting knifes, screw conveyors |