Allgemein
Property | Value |
---|---|
Dichte | 7.2 g/cm³ Show Supplier Material materials with Dichte of 7.2 g/cm³ |
Mechanisch
Property | Value |
---|---|
Elastizitätsmodul | 220 GPa Show Supplier Material materials with Elastizitätsmodul of 220 GPa |
Härte, Rockwell C | 60 - 63 [-] Show Supplier Material materials with Härte, Rockwell C of 60 - 63 [-] |
Chemical properties
Property | Value |
---|---|
Chrom | 5.3 % Show Supplier Material materials with Chrom of 5.3 % |
Eisen | Balance |
Kohlenstoff | 2.9 % Show Supplier Material materials with Kohlenstoff of 2.9 % |
Mangan | 0.5 % Show Supplier Material materials with Mangan of 0.5 % |
Molybdän | 1.3 % Show Supplier Material materials with Molybdän of 1.3 % |
Schwefel | 0.05 % Show Supplier Material materials with Schwefel of 0.05 % |
Silizium | 0.9 % Show Supplier Material materials with Silizium of 0.9 % |
Vanadium | 12 % Show Supplier Material materials with Vanadium of 12 % |
Technological properties
Property | ||
---|---|---|
Application areas | Various applications for cold work: punches, bending dies, cold forming presses, cutting knifes, screw conveyors |