Allgemein
Property | Value |
---|---|
Dichte | 7.1 g/cm³ Show Supplier Material materials with Dichte of 7.1 g/cm³ |
Mechanisch
Property | Value |
---|---|
Elastizitätsmodul | 220 GPa Show Supplier Material materials with Elastizitätsmodul of 220 GPa |
Härte, Rockwell C | 62 - 65 [-] Show Supplier Material materials with Härte, Rockwell C of 62 - 65 [-] |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Chrom | 13 % Show Supplier Material materials with Chrom of 13 % | ||
Eisen | Balance | ||
Kobalt | 0.5 % Show Supplier Material materials with Kobalt of 0.5 % | Ni+Co+W | |
Kohlenstoff | 4.4 % Show Supplier Material materials with Kohlenstoff of 4.4 % | ||
Mangan | 0.9 % Show Supplier Material materials with Mangan of 0.9 % | ||
Molybdän | 1.2 % Show Supplier Material materials with Molybdän of 1.2 % | ||
Nickel | 0.5 % Show Supplier Material materials with Nickel of 0.5 % | Ni+Co+W | |
Silizium | 0.9 % Show Supplier Material materials with Silizium of 0.9 % | ||
Vanadium | 15 % Show Supplier Material materials with Vanadium of 15 % | ||
Wolfram | 0.5 % Show Supplier Material materials with Wolfram of 0.5 % | Ni+Co+W |
Technological properties
Property | ||
---|---|---|
Application areas | Various applications for cold work: punches, bending dies, cold forming presses, cutting knifes; screw conveyors; knifes for the food industry |