Allgemein
Property | Value |
---|---|
Dichte | 8 g/cm³ Show Supplier Material materials with Dichte of 8 g/cm³ |
Mechanisch
Property | Value |
---|---|
Elastizitätsmodul | 230 GPa Show Supplier Material materials with Elastizitätsmodul of 230 GPa |
Härte, Rockwell C | 58 - 65 [-] Show Supplier Material materials with Härte, Rockwell C of 58 - 65 [-] |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100 °C | 1.15e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.15e-05 1/K | for 20°C to the mentioned temperature |
200 °C | 1.17e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.17e-05 1/K | for 20°C to the mentioned temperature | |
300 °C | 1.22e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.22e-05 1/K | for 20°C to the mentioned temperature | |
400 °C | 1.24e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.24e-05 1/K | for 20°C to the mentioned temperature | |
500 °C | 1.27e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.27e-05 1/K | for 20°C to the mentioned temperature | |
600 °C | 1.3e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.3e-05 1/K | for 20°C to the mentioned temperature | |
700 °C | 1.29e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.29e-05 1/K | for 20°C to the mentioned temperature | |
Spezifische Wärmekapazität | 420 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 420 J/(kg·K) | ||
Wärmeleitfähigkeit | 20 °C | 24.3 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 24.3 W/(m·K) |
Elektrisch
Property | Value |
---|---|
spezifischer Widerstand | 5.4e-07 Ω·m Show Supplier Material materials with spezifischer Widerstand of 5.4e-07 Ω·m |
Chemical properties
Property | Value |
---|---|
Chrom | 4.2 % Show Supplier Material materials with Chrom of 4.2 % |
Eisen | Balance |
Kohlenstoff | 1.3 % Show Supplier Material materials with Kohlenstoff of 1.3 % |
Molybdän | 5 % Show Supplier Material materials with Molybdän of 5 % |
Vanadium | 3 % Show Supplier Material materials with Vanadium of 3 % |
Wolfram | 6.4 % Show Supplier Material materials with Wolfram of 6.4 % |
Technological properties
Property | ||
---|---|---|
Application areas | Thread-cutting tools, reamers, heavy-duty milling cutters, drills, punching tools |