1.3294/1.3244 (HS6-5-3-8) high speed tool Co alloyed steel, with very good red hardness and tempering resistance .

Equivalent Materials

Ashby charts

See where Rapidur PM-30 falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Eigenschaften

Allgemein

Density

ρ

8.1 g/cm³ at 20 °C

Mechanisch

Elastic modulus

E

240 GPa at 20 °C

Hardness, Rockwell C

HRC

60 - 68 [-] at 20 °C

Thermisch

Coefficient of thermal expansion

α

1E-5 1/K at 100 °C

for 20°C to the mentioned temperature

Grafik verstecken

Specific heat capacity

cp

420 J/(kg·K) at 20 °C

Thermal conductivity

λ

22.2 W/(m·K) at 20 °C

Elektrisch

Electrical resistivity

ρel

6.1E-7 Ω·m at 20 °C

Chemische Eigenschaften

Element

Gew. %

Kommentar

Fe

-

Balance

Co

8.5 %

W

6.4 %

Mo

5 %

Cr

4.2 %

Mehr

Technische Eigenschaften

Application areas

Thread-cutting tools, reamers, heavy-duty milling cutters, drills, punching tools

Do you need more data regarding this material?

Diese Materialdaten wurden von Deutsche Edelstahlwerke Specialty Steel (DEW) zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.