Allgemein
Property | Value |
---|---|
Dichte | 8.2 g/cm³ Show Supplier Material materials with Dichte of 8.2 g/cm³ |
Mechanisch
Property | Value |
---|---|
Elastizitätsmodul | 241 GPa Show Supplier Material materials with Elastizitätsmodul of 241 GPa |
Härte, Rockwell C | 62 - 68 [-] Show Supplier Material materials with Härte, Rockwell C of 62 - 68 [-] |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100 °C | 1e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1e-05 1/K | for 20°C to the mentioned temperature |
200 °C | 1.05e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.05e-05 1/K | for 20°C to the mentioned temperature | |
300 °C | 1.08e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.08e-05 1/K | for 20°C to the mentioned temperature | |
400 °C | 1.12e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.12e-05 1/K | for 20°C to the mentioned temperature | |
500 °C | 1.13e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.13e-05 1/K | for 20°C to the mentioned temperature | |
600 °C | 1.14e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.14e-05 1/K | for 20°C to the mentioned temperature | |
700 °C | 1.16e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.16e-05 1/K | for 20°C to the mentioned temperature | |
Spezifische Wärmekapazität | 420 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 420 J/(kg·K) | ||
Wärmeleitfähigkeit | 20 °C | 20.5 - 24.6 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 20.5 - 24.6 W/(m·K) |
Elektrisch
Property | Value |
---|---|
spezifischer Widerstand | 6.1e-07 Ω·m Show Supplier Material materials with spezifischer Widerstand of 6.1e-07 Ω·m |
Chemical properties
Property | Value |
---|---|
Chrom | 5 % Show Supplier Material materials with Chrom of 5 % |
Eisen | Balance |
Kobalt | 8 % Show Supplier Material materials with Kobalt of 8 % |
Kohlenstoff | 1.6 % Show Supplier Material materials with Kohlenstoff of 1.6 % |
Molybdän | 2 % Show Supplier Material materials with Molybdän of 2 % |
Vanadium | 5 % Show Supplier Material materials with Vanadium of 5 % |
Wolfram | 10.5 % Show Supplier Material materials with Wolfram of 10.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Thread-cutting tools, heavy-duty milling cutters, drills for difficult to machine materials |