Abmessung
Mechanisch
Property | Value |
---|---|
Elastizitätsmodul | 206 GPa Show Supplier Material materials with Elastizitätsmodul of 206 GPa |
Härte, Rockwell C | 36 - 40 [-] Show Supplier Material materials with Härte, Rockwell C of 36 - 40 [-] |
Zugfestigkeit | 1125 - 1255 MPa Show Supplier Material materials with Zugfestigkeit of 1125 - 1255 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100 °C | 1.26e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.26e-05 1/K | for 20°C to the mentioned temperature |
150 °C | 1.28e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.28e-05 1/K | for 20°C to the mentioned temperature | |
200 °C | 1.3e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.3e-05 1/K | for 20°C to the mentioned temperature | |
250 °C | 1.33e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.33e-05 1/K | for 20°C to the mentioned temperature | |
300 °C | 1.35e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.35e-05 1/K | for 20°C to the mentioned temperature | |
350 °C | 1.37e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.37e-05 1/K | for 20°C to the mentioned temperature | |
400 °C | 1.39e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.39e-05 1/K | for 20°C to the mentioned temperature | |
450 °C | 1.4e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.4e-05 1/K | for 20°C to the mentioned temperature | |
500 °C | 1.42e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.42e-05 1/K | for 20°C to the mentioned temperature | |
Wärmeleitfähigkeit | 23 °C | 25.7 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 25.7 W/(m·K) | |
150 °C | 29.4 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 29.4 W/(m·K) | ||
300 °C | 29.8 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 29.8 W/(m·K) | ||
350 °C | 29.6 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 29.6 W/(m·K) | ||
400 °C | 29.2 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 29.2 W/(m·K) | ||
500 °C | 28.2 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 28.2 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Aluminium | 1 % Show Supplier Material materials with Aluminium of 1 % |
Eisen | Balance |
Kohlenstoff | 0.15 % Show Supplier Material materials with Kohlenstoff of 0.15 % |
Mangan | 1.5 % Show Supplier Material materials with Mangan of 1.5 % |
Nickel | 3 % Show Supplier Material materials with Nickel of 3 % |
Silizium | 0.3 % Show Supplier Material materials with Silizium of 0.3 % |
Technological properties
Property | ||
---|---|---|
Application areas | Suitable for all kinds of tools in plastic processing with high demands on strength, such as highly stressed plastic injection moulds, compression moulds, hot-runner. | |
Heat Treatment | Formadur PH 42 Superclean is supplied in precipitation hardened condition with a hardness of approx. 38 HRC. No additional heat treatment is necessary. After repair welding an ageing at 520 °C/1 hr is recommended. |