Allgemein
Property | Value |
---|---|
Partikelgrößenbereich | 10 - 53 µm Show Supplier Material materials with Partikelgrößenbereich of 10 - 53 µm |
Schüttdichte | 3.8 - 4.6 g/cm³ Show Supplier Material materials with Schüttdichte of 3.8 - 4.6 g/cm³ |
Mechanisch
Property | Value | Comment |
---|---|---|
Charpy impact energy, V-notch | 165 J Show Supplier Material materials with Charpy impact energy, V-notch of 165 J | |
Dehnung | 45 % Show Supplier Material materials with Dehnung of 45 % | A5 |
Streckgrenze | 440 - 540 MPa Show Supplier Material materials with Streckgrenze of 440 - 540 MPa | RP02 |
Zugfestigkeit | 520 - 620 MPa Show Supplier Material materials with Zugfestigkeit of 520 - 620 MPa |
Magnetisch
Property | Value | Comment |
---|---|---|
Relative magnetische Permeabilität | 1 [-] Show Supplier Material materials with Relative magnetische Permeabilität of 1 [-] | max. | None magnetic |
Rheological Properties
Property | Value |
---|---|
Halldurchfluss | 12 - 20 s/50g Show Supplier Material materials with Halldurchfluss of 12 - 20 s/50g |
Chemical properties
Property | Value |
---|---|
Chrom | 17 % Show Supplier Material materials with Chrom of 17 % |
Eisen | Balance |
Kohlenstoff | 0.03 % Show Supplier Material materials with Kohlenstoff of 0.03 % |
Mangan | 1 % Show Supplier Material materials with Mangan of 1 % |
Molybdän | 2 % Show Supplier Material materials with Molybdän of 2 % |
Nickel | 13 % Show Supplier Material materials with Nickel of 13 % |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Additive manufacturing | |
Corrosion properties | In printed condition Prindur® 4404 is corrosion resistant according to SEP 1877 Method II (intergranular corrosion resistance test) and ASTM G48 Method E (pitting corrosion resistance test). | |
Processing history | The powder is produced by gas atomization. | |
Processing methods | Printdur® 4404 can be processed on LPBF systems. The process parameters are similar to those of 1.4404/316L. |