Allgemein
Property | Value |
---|---|
Partikelgrößenbereich | 20 - 53 µm Show Supplier Material materials with Partikelgrößenbereich of 20 - 53 µm |
Schüttdichte | 3.8 - 4.6 g/cm³ Show Supplier Material materials with Schüttdichte of 3.8 - 4.6 g/cm³ |
Mechanisch
Property | Value | Comment |
---|---|---|
Charpy impact energy, V-notch | 100 J Show Supplier Material materials with Charpy impact energy, V-notch of 100 J | |
Dehnung | 35 % Show Supplier Material materials with Dehnung of 35 % | A5 |
Streckgrenze | 660 - 760 MPa Show Supplier Material materials with Streckgrenze of 660 - 760 MPa | RP02 |
Zugfestigkeit | 920 - 1030 MPa Show Supplier Material materials with Zugfestigkeit of 920 - 1030 MPa |
Magnetisch
Property | Value | Comment |
---|---|---|
Relative magnetische Permeabilität | 1 [-] Show Supplier Material materials with Relative magnetische Permeabilität of 1 [-] | max. | None magnetic |
Rheological Properties
Property | Value |
---|---|
Halldurchfluss | 12 - 20 s/50g Show Supplier Material materials with Halldurchfluss of 12 - 20 s/50g |
Chemical properties
Property | Value |
---|---|
Chrom | 22 % Show Supplier Material materials with Chrom of 22 % |
Eisen | 5 % Show Supplier Material materials with Eisen of 5 % |
Kobalt | 0.5 % Show Supplier Material materials with Kobalt of 0.5 % |
Kohlenstoff | 0.03 % Show Supplier Material materials with Kohlenstoff of 0.03 % |
Mangan | 0.5 % Show Supplier Material materials with Mangan of 0.5 % |
Molybdän | 9 % Show Supplier Material materials with Molybdän of 9 % |
Nickel | Balance |
Niobium | 3.5 % Show Supplier Material materials with Niobium of 3.5 % |
Silizium | 0.5 % Show Supplier Material materials with Silizium of 0.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Additive manufacturing | |
Processing history | The powder is produced by gas atomization. | |
Processing methods | Printdur® Ni625 can be processed on LPBF systems. The process parameters are similar to those of alloy 625. Please contact us for further information. |