Allgemein
Property | Value |
---|---|
Dichte | 7.9 g/cm³ Show Supplier Material materials with Dichte of 7.9 g/cm³ |
Partikelgrößenbereich | 10 - 45 µm Show Supplier Material materials with Partikelgrößenbereich of 10 - 45 µm |
Schüttdichte | 4.63 g/cm³ Show Supplier Material materials with Schüttdichte of 4.63 g/cm³ |
Mechanisch
Property | Value | Comment |
---|---|---|
Charpy impact energy, V-notch | 22 J Show Supplier Material materials with Charpy impact energy, V-notch of 22 J | |
Dehnung | 27 % Show Supplier Material materials with Dehnung of 27 % | A5 |
Härte, Rockwell C | 27 [-] Show Supplier Material materials with Härte, Rockwell C of 27 [-] | |
Streckgrenze | 630 MPa Show Supplier Material materials with Streckgrenze of 630 MPa | RP02 |
Zugfestigkeit | 1080 MPa Show Supplier Material materials with Zugfestigkeit of 1080 MPa |
Thermisch
Property | Value |
---|---|
Koeffizient der thermischen Ausdehnung | 1.05e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.05e-05 1/K |
Rheological Properties
Property | Value |
---|---|
Halldurchfluss | 16 s/50g Show Supplier Material materials with Halldurchfluss of 16 s/50g |
Chemical properties
Property | Value |
---|---|
Chrom | 28 % Show Supplier Material materials with Chrom of 28 % |
Eisen | 0.75 % Show Supplier Material materials with Eisen of 0.75 % |
Kobalt | Balance |
Kohlenstoff | 0.14 % Show Supplier Material materials with Kohlenstoff of 0.14 % |
Mangan | 1 % Show Supplier Material materials with Mangan of 1 % |
Molybdän | 6 % Show Supplier Material materials with Molybdän of 6 % |
Nickel | 0.1 % Show Supplier Material materials with Nickel of 0.1 % |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % |
Stickstoff | 0.25 % Show Supplier Material materials with Stickstoff of 0.25 % |
Technological properties
Property | ||
---|---|---|
Application areas | Suitable for the production of CoCrMo implants | |
Processing history | The powder is produced by gas atomization. | |
Processing methods | Printdur® CoCrF75 can be processed on LPBF systems. |