Allgemein
Property | Value |
---|---|
Partikelgrößenbereich | 10 - 53 µm Show Supplier Material materials with Partikelgrößenbereich of 10 - 53 µm |
Schüttdichte | 4.3 g/cm³ Show Supplier Material materials with Schüttdichte of 4.3 g/cm³ |
Mechanisch
Property | Value | Comment |
---|---|---|
Charpy impact energy, V-notch | 50 J Show Supplier Material materials with Charpy impact energy, V-notch of 50 J | |
Dehnung | 30 % Show Supplier Material materials with Dehnung of 30 % | A5 |
Härte, Rockwell C | 35 [-] Show Supplier Material materials with Härte, Rockwell C of 35 [-] | |
Streckgrenze | 915 MPa Show Supplier Material materials with Streckgrenze of 915 MPa | RP02 |
Zugfestigkeit | 1120 MPa Show Supplier Material materials with Zugfestigkeit of 1120 MPa |
Magnetisch
Property | Value | Comment |
---|---|---|
Relative magnetische Permeabilität | 1 [-] Show Supplier Material materials with Relative magnetische Permeabilität of 1 [-] | max. | None magnetic |
Rheological Properties
Property | Value |
---|---|
Halldurchfluss | 16.8 s/50g Show Supplier Material materials with Halldurchfluss of 16.8 s/50g |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Chrom | 18 % Show Supplier Material materials with Chrom of 18 % | ||
Eisen | Balance | ||
Kohlenstoff | 1 % Show Supplier Material materials with Kohlenstoff of 1 % | N+C | |
Mangan | 21 % Show Supplier Material materials with Mangan of 21 % | ||
Molybdän | 2 % Show Supplier Material materials with Molybdän of 2 % | ||
Nickel | 0.1 % Show Supplier Material materials with Nickel of 0.1 % | ||
Stickstoff | 1 % Show Supplier Material materials with Stickstoff of 1 % | N+C |
Technological properties
Property | ||
---|---|---|
Application areas | The properties of Printdur® HSA offer a wide range of applications in mechanical engineering, e.g. food and chemical industry, pump components, the power plant industry or the automotive industy. | |
Corrosion properties | In printed condition Prindur® HSA is corrosion resistant according to SEP 1877 Method II (intergranular corrosion resistance test) and ASTM G48 Method E (pitting corrosion resistance test). | |
Processing history | The powder is produced by gas atomization. | |
Processing methods | Printdur® HSA can be processed on LPBF systems. The process parameters are similar to those of 316L. Please contact us for further information. |