Mechanisch
Property | Value | Comment |
---|---|---|
Charpy impact energy, V-notch | 40 J Show Supplier Material materials with Charpy impact energy, V-notch of 40 J | |
Dehnung | 10 % Show Supplier Material materials with Dehnung of 10 % | A5 |
Härte, Rockwell C | 44 [-] Show Supplier Material materials with Härte, Rockwell C of 44 [-] | |
Streckgrenze | 1220 MPa Show Supplier Material materials with Streckgrenze of 1220 MPa | RP02 |
Zugfestigkeit | 1500 MPa Show Supplier Material materials with Zugfestigkeit of 1500 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 1 % Show Supplier Material materials with Chrom of 1 % |
Kohlenstoff | 0.22 % Show Supplier Material materials with Kohlenstoff of 0.22 % |
Mangan | 1.4 % Show Supplier Material materials with Mangan of 1.4 % |
Molybdän | 1 % Show Supplier Material materials with Molybdän of 1 % |
Silizium | 0.8 % Show Supplier Material materials with Silizium of 0.8 % |
Technological properties
Property | ||
---|---|---|
Application areas | Additive Manufacturing | |
Processing history | The powder is produced by gas atomization. | |
Processing methods | Bainidur® AM can be processed on LPBF systems |