Allgemein
Property | Value |
---|---|
Dichte | 7.7 g/cm³ Show Supplier Material materials with Dichte of 7.7 g/cm³ |
Abmessung
Property | Value | Comment |
---|---|---|
Durchmesser | 250 mm Show Supplier Material materials with Durchmesser of 250 mm | max. |
Mechanisch
Property | Value | Comment |
---|---|---|
Charpy impact energy, V-notch | 35 J Show Supplier Material materials with Charpy impact energy, V-notch of 35 J | |
Dehnung | 10 - 14 % Show Supplier Material materials with Dehnung of 10 - 14 % | A5 |
Elastizitätsmodul | 210 GPa Show Supplier Material materials with Elastizitätsmodul of 210 GPa | |
Flächenreduzierung | 40 - 55 % Show Supplier Material materials with Flächenreduzierung of 40 - 55 % | |
Härte, Brinell | 195 - 300 [-] Show Supplier Material materials with Härte, Brinell of 195 - 300 [-] | Depending on the delivery condition |
Streckgrenze | 500 - 900 MPa Show Supplier Material materials with Streckgrenze of 500 - 900 MPa | |
Zugfestigkeit | 750 - 1300 MPa Show Supplier Material materials with Zugfestigkeit of 750 - 1300 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100 °C | 1.11e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.11e-05 1/K | for 20°C to the mentioned temperature |
200 °C | 1.21e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.21e-05 1/K | for 20°C to the mentioned temperature | |
300 °C | 1.29e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.29e-05 1/K | for 20°C to the mentioned temperature | |
400 °C | 1.35e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.35e-05 1/K | for 20°C to the mentioned temperature | |
Spezifische Wärmekapazität | 470 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 470 J/(kg·K) | ||
Wärmeleitfähigkeit | 42.6 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 42.6 W/(m·K) |
Elektrisch
Property | Value |
---|---|
spezifischer Widerstand | 1.9e-07 Ω·m Show Supplier Material materials with spezifischer Widerstand of 1.9e-07 Ω·m |
Chemical properties
Property | Value |
---|---|
Chrom | 0.9 - 1.2 % Show Supplier Material materials with Chrom of 0.9 - 1.2 % |
Eisen | Balance |
Kohlenstoff | 0.38 - 0.45 % Show Supplier Material materials with Kohlenstoff of 0.38 - 0.45 % |
Mangan | 0.6 - 0.99 % Show Supplier Material materials with Mangan of 0.6 - 0.99 % |
Molybdän | 0.15 - 0.3 % Show Supplier Material materials with Molybdän of 0.15 - 0.3 % |
Phosphor | 0.025 % Show Supplier Material materials with Phosphor of 0.025 % |
Schwefel | 0.035 % Show Supplier Material materials with Schwefel of 0.035 % |
Silizium | 0.4 % Show Supplier Material materials with Silizium of 0.4 % |
Technological properties
Property | ||
---|---|---|
Application areas | It is mainly used in automotive and vehicle construction for highly stressed components, such as steering knuckles, connecting rods, crankshafts, gear shafts, gears or pinions. | |
Heat Treatment | Normalizing 840-880°C (Air), Soft annealing: 680-720°C (Oven, slow cooling), Quenching: 820-860°C (Oil, Water), Tempering: 540-680°C (Air) | |
Hot forming | It is formable at 850-1100°C. | |
Processing history | Quenched and Tempered | |
Welding | It is difficult to weld and should will not used be in welded constructions. If welding is not an issue, the demanding requirements of welding filler by material manufacturers must be taken into account.. The main temperature is increased by heat treatment to equalize the structural condition. |