Allgemein
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dichte | 1.43 g/cm³ Show Supplier Material materials with Dichte of 1.43 g/cm³ | ||
Schüttdichte | 0.8 g/cm³ Show Supplier Material materials with Schüttdichte of 0.8 g/cm³ | EN ISO 60 | |
Wasserabsorption | 2 % Show Supplier Material materials with Wasserabsorption of 2 % | DIN EN ISO 62 | 23°C | 50 % r.h. up to saturation |
Mechanisch
Property | Value | Testing Standard |
---|---|---|
Biegefestigkeit | 90 MPa Show Supplier Material materials with Biegefestigkeit of 90 MPa | DIN EN ISO 178 |
Biegemodul | 2.8 GPa Show Supplier Material materials with Biegemodul of 2.8 GPa | DIN EN ISO 178 |
Dehnung | 10.8 % Show Supplier Material materials with Dehnung of 10.8 % | DIN EN ISO 527-1 |
Elastizitätsmodul | 3.2 GPa Show Supplier Material materials with Elastizitätsmodul of 3.2 GPa | DIN EN ISO 527-1 |
Flexural strain | 5.5 % Show Supplier Material materials with Flexural strain of 5.5 % | DIN EN ISO 178 |
Schlagzähigkeit, Charpy ungekerbt | 84 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 84 kJ/m² | DIN EN ISO 179-1eU |
Zugfestigkeit | 60 MPa Show Supplier Material materials with Zugfestigkeit of 60 MPa | DIN EN ISO 527-1 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Glasübergangstemperatur | 72 °C Show Supplier Material materials with Glasübergangstemperatur of 72 °C | ||
Max. Betriebstemperatur | 110 °C Show Supplier Material materials with Max. Betriebstemperatur of 110 °C | Long | |
170 °C Show Supplier Material materials with Max. Betriebstemperatur of 170 °C | Short | ||
Schmelzpunkt | 260 °C Show Supplier Material materials with Schmelzpunkt of 260 °C | ||
Entflammbarkeit | UL94 class HB, DIN IEC 60695-11-10 |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 25 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 25 g/10min | DIN EN ISO 1133 | 280°C/2.16kg |
Schmelzvolumenflussrate | 21 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 21 cm³/10min | DIN EN ISO 1133 | 280°C/2.16kg |
Schrumpfung | 1.81 % Show Supplier Material materials with Schrumpfung of 1.81 % | DIN EN ISO 294-4 | |
2.26 % Show Supplier Material materials with Schrumpfung of 2.26 % | DIN EN ISO 294-4 | Transverse |
Technological properties
Property | ||
---|---|---|
Application areas | Food engineering | |
Certifications | Explanation of food contact according to FDA and EU 10/2011 | |
Color | Blue | |
Detectability | Inductive: 5.5 mm Al | |
Fillers | Detectable Filler | |
Processing methods | Permissible residual moisture content (%): 0.1, drying temperature (°C): 80, drying time (h): 8, mould temperature (°C): 150, material temperature (°C): 310, cylinder/processing temperature (°C): 310 |