Allgemein
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dichte | 1 g/cm³ Show Supplier Material materials with Dichte of 1 g/cm³ | ||
Schüttdichte | 0.57 g/cm³ Show Supplier Material materials with Schüttdichte of 0.57 g/cm³ | EN ISO 60 | |
Wasserabsorption | 0.1 % Show Supplier Material materials with Wasserabsorption of 0.1 % | DIN EN ISO 62 | max. | 23°C | 50 % r.h. up to saturation |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dehnung | 2.2 % Show Supplier Material materials with Dehnung of 2.2 % | DIN EN ISO 527-1 | |
Druckfestigkeit | 65.9 MPa Show Supplier Material materials with Druckfestigkeit of 65.9 MPa | EN ISO 604 | 1% |
Elastizitätsmodul | 0.0103 GPa Show Supplier Material materials with Elastizitätsmodul of 0.0103 GPa | DIN EN ISO 527-1 | |
Kompressionsmodul | 5810 GPa Show Supplier Material materials with Kompressionsmodul of 5810 GPa | EN ISO 604 | |
Schlagzähigkeit, Charpy ungekerbt | 23.6 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 23.6 kJ/m² | DIN EN ISO 179-1eU | |
Zugfestigkeit | 111 MPa Show Supplier Material materials with Zugfestigkeit of 111 MPa | DIN EN ISO 527-1 |
Thermisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Glasübergangstemperatur | 143 °C Show Supplier Material materials with Glasübergangstemperatur of 143 °C | ||
Koeffizient der thermischen Ausdehnung | 1.9e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.9e-05 1/K | DIN EN ISO 11359-1/2 | at 23-140°C |
3.8e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 3.8e-05 1/K | DIN EN ISO 11359-1/2 | at 180-285°C | |
Max. Betriebstemperatur | 260 °C Show Supplier Material materials with Max. Betriebstemperatur of 260 °C | Long | |
300 °C Show Supplier Material materials with Max. Betriebstemperatur of 300 °C | Short | ||
Schmelzpunkt | 343 °C Show Supplier Material materials with Schmelzpunkt of 343 °C |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 17.8 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 17.8 g/10min | DIN EN ISO 1133 | 380°C/5kg |
Schrumpfung | 0.39 % Show Supplier Material materials with Schrumpfung of 0.39 % | DIN EN ISO 294-4 | |
1.23 % Show Supplier Material materials with Schrumpfung of 1.23 % | DIN EN ISO 294-4 | Transverse |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive industry: Seat (bumper, roll), Steering, Gear (shift handle and bearings), electronics (radar) | |
Color | Gray | |
Fillers | Silicon Carbide | |
Processing methods | Permissible residual moisture content (%): 0.02, drying temperature (°C): 140-180, drying time (h): 4-6, mould temperature (°C): 160-200, material temperature (°C): 390-400, cylinder/processing temperature (°C): 360-400 |