Allgemein
Property | Value |
---|---|
Dichte | 1.42 g/cm³ Show Supplier Material materials with Dichte of 1.42 g/cm³ |
Mechanisch
Property | Value | Testing Standard |
---|---|---|
Dehnung | 9.5 % Show Supplier Material materials with Dehnung of 9.5 % | DIN EN ISO 527-1 |
Elastizitätsmodul | 1.1 GPa Show Supplier Material materials with Elastizitätsmodul of 1.1 GPa | DIN EN ISO 527-1 |
Schlagzähigkeit, Charpy ungekerbt | 28 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 28 kJ/m² | DIN EN ISO 179-1eU |
Zugfestigkeit | 18 MPa Show Supplier Material materials with Zugfestigkeit of 18 MPa | DIN EN ISO 527-1 |
Thermisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Glasübergangstemperatur | -100 °C Show Supplier Material materials with Glasübergangstemperatur of -100 °C | DIN 53765 | |
Max. Betriebstemperatur | 70 °C Show Supplier Material materials with Max. Betriebstemperatur of 70 °C | Long | |
100 °C Show Supplier Material materials with Max. Betriebstemperatur of 100 °C | Short | ||
Schmelzpunkt | 109 °C Show Supplier Material materials with Schmelzpunkt of 109 °C |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 11 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 11 g/10min | DIN EN ISO 1133 | 230°C/2.16kg |
Schrumpfung | 1.9 % Show Supplier Material materials with Schrumpfung of 1.9 % | DIN EN ISO 294-4 | |
3.5 % Show Supplier Material materials with Schrumpfung of 3.5 % | DIN EN ISO 294-4 | Transverse |
Technological properties
Property | ||
---|---|---|
Certifications | Explanation of food contact according to FDA and EU 10/2011 on request | |
Color | Blue | |
Detectability | Inductive: 6 mm Al | |
Fillers | Mineral Powder | |
Processing methods | Permissible residual moisture content (%): 0.1, drying temperature (°C): 80, drying time (h): 4, mould temperature (°C): 60, material temperature (°C): 240, cylinder/processing temperature (°C): 240 |