Allgemein
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dichte | 2.38 g/cm³ Show Supplier Material materials with Dichte of 2.38 g/cm³ | ||
Schüttdichte | 1.11 g/cm³ Show Supplier Material materials with Schüttdichte of 1.11 g/cm³ | EN ISO 60 | |
Wasserabsorption | 0.1 % Show Supplier Material materials with Wasserabsorption of 0.1 % | DIN EN ISO 62 | max. | 23°C | 50 % r.h. up to saturation |
Mechanisch
Property | Value | Testing Standard |
---|---|---|
Biegefestigkeit | 20 MPa Show Supplier Material materials with Biegefestigkeit of 20 MPa | DIN EN ISO 178 |
Biegemodul | 0.6 GPa Show Supplier Material materials with Biegemodul of 0.6 GPa | DIN EN ISO 178 |
Dehnung | 12 % Show Supplier Material materials with Dehnung of 12 % | DIN EN ISO 527-1 |
Elastizitätsmodul | 0.91 GPa Show Supplier Material materials with Elastizitätsmodul of 0.91 GPa | DIN EN ISO 527-1 |
Flexural strain | 12 % Show Supplier Material materials with Flexural strain of 12 % | DIN EN ISO 178 |
Schlagzähigkeit, Charpy ungekerbt | 60 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 60 kJ/m² | DIN EN ISO 179-1eU |
Zugfestigkeit | 14 MPa Show Supplier Material materials with Zugfestigkeit of 14 MPa | DIN EN ISO 527-1 |
Thermisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Glasübergangstemperatur | -100 °C Show Supplier Material materials with Glasübergangstemperatur of -100 °C | DIN 53765 | |
Max. Betriebstemperatur | 70 °C Show Supplier Material materials with Max. Betriebstemperatur of 70 °C | Long | |
100 °C Show Supplier Material materials with Max. Betriebstemperatur of 100 °C | Short | ||
Schmelzpunkt | 109 °C Show Supplier Material materials with Schmelzpunkt of 109 °C |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 12.4 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 12.4 g/10min | DIN EN ISO 1133 | 230°C/5kg |
Schmelzvolumenflussrate | 6.1 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 6.1 cm³/10min | DIN EN ISO 1133 | |
Schrumpfung | 1.6 % Show Supplier Material materials with Schrumpfung of 1.6 % | DIN EN ISO 294-4 | Transverse |
1.67 % Show Supplier Material materials with Schrumpfung of 1.67 % | DIN EN ISO 294-4 |
Technological properties
Property | ||
---|---|---|
Certifications | Explanation of food contact according to FDA and EU 10/2011 on request | |
Color | Black | |
Fillers | Detectable Filler | |
Processing methods | Permissible residual moisture content (%): 0.1, drying temperature (°C): 80, drying time (h): 44231, mould temperature (°C): 30-60, material temperature (°C): 200-240, cylinder/processing temperature (°C): 190-240 |